Synthesis, oxidation resistance, thermal stability and, mechanical properties of Ti$_{0.33-x}$Al$_{x}$B$_{y}$ coatings



Verantwortlichkeitsangabevorgelegt von Amir Hossein Navidi Kashani, M.Sc. RWTH, M.Sc.

ImpressumAachen : RWTH Aachen University 2024

Umfang1 Online-Ressource : Illustrationen


Dissertation, Rheinisch-Westfälische Technische Hochschule Aachen, 2024

Veröffentlicht auf dem Publikationsserver der RWTH Aachen University


Genehmigende Fakultät
Fak05

Hauptberichter/Gutachter
;

Tag der mündlichen Prüfung/Habilitation
2024-06-26

Online
DOI: 10.18154/RWTH-2024-06348
URL: https://publications.rwth-aachen.de/record/988667/files/988667.pdf

Einrichtungen

  1. Lehrstuhl für Werkstoffchemie (521110)
  2. Fachgruppe für Materialwissenschaft und Werkstofftechnik (520000)

Projekte

  1. DFG project 449548449 - Oxidationsverhalten von Ti1-yAlyB- und Ti1-xAlxN-Dünnschichten in Abhängigkeit von der Al-Konzentration (449548449) (449548449)

Inhaltliche Beschreibung (Schlagwörter)
AlB12 formation (frei) ; elastic modulus (frei) ; hard coatings (frei) ; oxidation (frei) ; spinodal decomposition (frei) ; stoichiometric (TiAl)B2 (frei) ; thermal stability (frei)

Thematische Einordnung (Klassifikation)
DDC: 620

Kurzfassung
Im ersten Teil dieser Arbeit wurde die Auswirkung der B-Konzentration auf die Phasenbildung und die Oxidationsbeständigkeit von (Ti0.35Al0.65)By-Beschichtungen mit y = 1.7, 2.0, 2.4 untersucht. Elementare B-Targets wurden im RF-Modus und ein Ti0.4Al0.6-Target wurde im DC-Modus gesputtert. Die B-Konzentration wurde systematisch variiert, indem die dem jeweiligen Magnetron zugeführte Leistung angepasst wurde, während die mit dem Ti0.4Al0.6-Target zugeführte Leistung konstant gehalten wurde. Die gemessenen Gitterparameter und elastischen Eigenschaften stimmen mit den ab-initio-Vorhersagen überein. Die Oxidationsbeständigkeit bei 700 °C in Luft für bis zu 8 Stunden wurde mit einer mittels kathodischer Lichtbogenverdampfung hergestellten (Ti0.37Al0.63)0.49N0.51 -Beschichtung mit einem Al/Ti-Verhältnis von 1.69 ± 0.20 verglichen, ähnlich zu 1.84 ± 0.40 für die Boridbeschichtungen. Rastertransmissionselektronenmikroskopische (STEM) Aufnahmen ergaben nach 8 Stunden Oxidschichtdicken von 39 ± 7 und 101 ± 25 nm für (Ti0.35Al0.65)B2.0 und (Ti0.37Al0.63)0.49N0.51. Das nahezu stöchiometrische Diborid zeigt somit eine im Vergleich zur Nitridbeschichtung höhere Oxidationsbeständigkeit. Dieses Verhalten lässt sich anhand der Zusammensetzung und Strukturanalyse der Oxidschichten erklären: Während die Schutzschicht auf dem Diborid hauptsächlich aus Al und O besteht, enthält die poröse Oxidschicht auf der Nitridschicht Ti, Al und O. Im zweiten Teil der Arbeit wird der Einfluss des Aluminium-Gehalts auf die Phasenbildung, die mechanischen Eigenschaften und das Oxidationsverhalten von stöchiometrischen Ti0.33-xAlxB0.67 (x = 0.04, 0.15, 0.21, und 0.28) Schutzschichten untersucht. Das mittels Röntgendiffraktometrie ermittelte experimentelle Einheitszellenvolumen und der durch Nanoindentation gemessene Elastizitätsmodul der Beschichtungen, die in guter Übereinstimmung mit den ab-initio-Vorhersagen sind, zeigen eine merkliche Abnahme mit zunehmendem Al-Gehalt. Die Analyse mittels STEM ergab ein bimodales, stark von der Al-Konzentration abhängiges Oxidationsverhalten, bei dem Schichten mit einem Al-Gehalt von ≤ 15 At.-% eine poröse, nicht passivierende kristalline Oxidschicht bilden, die sowohl Ti-reiche als auch Al-reiche Oxidbereiche enthält, während bei Schichten mit einem Al-Gehalt von ≥ 21 At.-% die Bildung einer passivierenden, dichten, röntgenamorphen Oxidschicht beobachtet wurde. Zeitgleich mit der passivierenden Schichtbildung für Al-Konzentrationen ≥ 21 At.-% sinkt das Elastizitätsmodul im Vergleich zu TiB2 um ≥ 32.6 %, was auf eine durch die Al-Konzentration induzierte Bindungsschwächung zurückgeführt werden kann, wie die damit einhergehende Verringerung der Kohäsionsenergie um ≥ 22 % zeigt. Im dritten und letzten Teil der Arbeit wird die thermische Stabilität von stöchiometrischem Ti0.12Al0.21B0.67 durch Vakuumglühen für 1 und 3 Stunden bei 1000 °C untersucht. Die Beschichtungen im Ausgangszustand und nach dem Glühen wurden hinsichtlich der Veränderungen in der chemischen Zusammensetzung, der Phasenbildung und der Morphologie verglichen. Röntgenbeugungsdaten deuten auf die Bildung eines einphasigen Mischkristalls in den Ti0.12Al0.21B0.67-Dünnschichten im Ausgangszustand hin. Nach einer 1-stündigen Glühung zeigen Untersuchungen mittels STEM, energiedispersive Röntgenspektroskopie und Atomsondentomographie eine Entmischung in Al- und Ti-reiche (Ti,Al)B2-Domänen, was mit einer spinodalen Zersetzung übereinstimmt. Darüber hinaus deutet die Bildung von AlB12 mit einer gleichzeitigen Verringerung der Al-Konzentration von 20.9 auf 16.8 At.-%, wahrscheinlich durch Verdampfung, auf die Zersetzung der Al-reichen (Ti,Al)B2-Domänen während des Glühens für 1 h hin. Die Analyse der Probe nach 3-stündigem Glühen zeigt Hinweise auf eine fortgesetzte spinodale Zersetzung sowie auf eine weitere Zersetzung von Al-reichen (Ti,Al)B2-Domänen, die neben der Bildung von AlB12 zu einer Verringerung der Al-Konzentration auf 12.5 At.-% durch Al-Verdampfung führt. Der Trend zur Phasenbildung, der bei in situ-TEM-Studien bei 1100 °C beobachtet wurde, stimmt mit den oben beschriebenen Zersetzungsprozessen überein. Die hier ermittelte thermische Stabilitätsgrenze, die mittels räumlich aufgelöster Struktur- und Zusammensetzungsanalyse aufgedeckt wurde, begrenzt den Anwendungstemperaturbereich von Ti0.12Al0.21B0.67 im Vakuum auf Temperaturen < 1000 °C und unterstreicht, dass thermische Stabilitätsuntersuchungen, die ausschließlich auf Röntgenbeugungsdaten beruhen, zu einer Überschätzung thermischen Stabilität führen.

In the first part of this thesis, the effect of B concentration on phase formation and oxidation resistance of (Ti0.35Al0.65)By coatings with y = 1.7, 2.0, 2.4 was investigated. Elemental B targets in radio frequency mode and a compound Ti0.4Al0.6 target in direct current mode were sputtered. The B concentration was varied systematically by adjusting the applied power to the respective magnetrons while keeping the power supplied to the magnetron with the Ti0.4Al0.6 target constant. Measured lattice parameters and elastic properties are consistent with ab initio predictions. The oxidation resistance at 700 °C in air for up to 8 h was compared to a cathodic arc evaporated (Ti0.37Al0.63)0.49N0.51 coating with an Al/Ti ratio of 1.69 ± 0.20 which is very similar to 1.84 ± 0.40 for the boride coatings. Scanning transmission electron microscopy imaging revealed oxide scale thicknesses of 39 ± 7 and 101 ± 25 nm for (Ti0.35Al0.65)B2.0 and (Ti0.37Al0.63)0.49N0.51 after 8 h, respectively. Hence, the close to stoichiometric diboride outperforms the nitride coating. This behavior can be understood based on composition and structure analysis of the oxide scales: While the protective layer on the diboride is primarily composed of Al and O, the porous oxide layer on the nitride coating contains Ti, Al and O. In the second part, the impact of Al concentration on phase formation, mechanical properties, and oxidation behavior of stoichiometric Ti0.33-xAlxB0.67 with x = 0.04, 0.15, 0.21, and 0.28 is investigated. The experimental unit cell volume, obtained from X-ray diffractograms, and elastic modulus, measured by nanoindentation, of as-deposited coatings which are in good agreement with ab initio predictions exhibit a noticeable decline with increasing Al concentration. Analysis by scanning transmission electron microscopy revealed a bimodal, strongly Al concentration-dependent oxidation behavior where films containing ≤ 15 at. % of Al form a porous, non-passivating crystalline oxide scale containing Ti-rich as well as Al-rich oxide regions, while the formation of a passivating, dense, X-ray amorphous oxide scale was observed for films containing ≥ 21 at. % of Al. Coincident with the passive scale formation for Al concentrations ≥ 21 at. %, the elastic modulus decreases by ≥ 32.6 % compared to TiB2 and can be rationalized based on Al concentration-induced bond weakening as revealed by the concomitant cohesive energy reduction of ≥ 22 %. In the third and last part, the thermal stability of stoichiometric Ti0.12Al0.21B0.67 is explored by vacuum annealing at 1000 °C for 1 and 3 hours. The as-deposited and post-annealed coatings were compared regarding changes in chemical composition, phase formation, and morphology. X-ray diffraction data indicate the formation of a single-phase solid solution in the as-deposited Ti0.12Al0.21B0.67 thin films. After annealing for 1 h, scanning transmission electron microscopy, energy-dispersive X-ray mapping, and atom probe tomography investigations reveal segregation into Al- and Ti-rich (Ti,Al)B2 domains, consistent with spinodal decomposition. Furthermore, the formation of AlB12 with a concomitant reduction in Al concentration from 20.9 to 16.8 at. %, likely by evaporation, indicate the decomposition of Al-rich (Ti,Al)B2 domains during annealing for 1 h. Analysis of the sample after annealing for 3 h shows evidence for continued spinodal decomposition as well as for further decomposition of Al-rich (Ti,Al)B2 domains, leading besides the formation of AlB12 to a reduction in Al concentration to 12.5 at. % by Al evaporation. The observed phase formation trend during in-situ TEM studies at 1100 °C is consistent with the above discussed decomposition processes. The here identified thermal stability limit, revealed with spatially resolved structure and composition probes, confines the application temperature range of Ti0.12Al0.21B0.67 in vacuum to temperatures < 1000 °C and underlines that thermal stability investigations solely based on X-ray diffraction data result in an overestimated thermal stability.

OpenAccess:
Download fulltext PDF
(additional files)

Dokumenttyp
Dissertation / PhD Thesis

Format
online

Sprache
English

Externe Identnummern
HBZ: HT030801099

Interne Identnummern
RWTH-2024-06348
Datensatz-ID: 988667

Beteiligte Länder
Germany

 GO


Related:

http://join2-wiki.gsi.de/foswiki/pub/Main/Artwork/join2_logo100x88.png Journal Article/Contribution to a book  ;  ;  ;  ;  ;  ;  ;
Synthesis and oxidation behavior of Ti0.35Al0.65By (y = 1.7–2.4) coatings
Surface and coatings technology 442, 128190 () [10.1016/j.surfcoat.2022.128190] special issue: "Special Issue of Surface and Coatings Technology celebrating the pioneering research career of Professor Allan Matthews in the field of "Plasma-based Surface Engineering""  GO BibTeX | EndNote: XML, Text | RIS

http://join2-wiki.gsi.de/foswiki/pub/Main/Artwork/join2_logo100x88.png Journal Article  ;  ;  ;  ;  ;  ;  ;  ;
Morphology, mechanical properties, and oxidation behavior of stoichiometric Ti0.33-xAlxB0.67 coatings (x = 0.04, 0.15, 0.21, and 0.28)
Acta materialia 270, 119829 () [10.1016/j.actamat.2024.119829]  GO OpenAccess  Download fulltext Files BibTeX | EndNote: XML, Text | RIS

http://join2-wiki.gsi.de/foswiki/pub/Main/Artwork/join2_logo100x88.png Journal Article  ;  ;  ;  ;  ;  ;  ;  ;  ;
Temporally-resolved decomposition of Ti0.12Al0.21B0.67 thin films at 1000 °C
Surface and coatings technology 487, 131026 () [10.1016/j.surfcoat.2024.131026]  GO OpenAccess  Download fulltext Files BibTeX | EndNote: XML, Text | RIS


OpenAccess

QR Code for this record

The record appears in these collections:
Document types > Theses > Ph.D. Theses
Faculty of Georesources and Materials Engineering (Fac.5) > Division of Materials Science and Engineering
Publication server / Open Access
Public records
Publications database
520000
521110

 Record created 2024-07-04, last modified 2025-09-30


OpenAccess:
Download fulltext PDF
(additional files)
Rate this document:

Rate this document:
1
2
3
 
(Not yet reviewed)